MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Wall Colmonoy COLMONOY® 83 PTA Nickel-Chromium-Boron Matrix Alloy With Tungsten Carbide
Categories: Metal; Metal Matrix Composite; Nonferrous Metal; Nickel Alloy; Tungsten Alloy

Material Notes: A tough nickel-chromium-tungsten-boron matrix alloy containing chromium carbides with the addition of extremely hard tungsten-carbide particles for excellent abrasive wear protection. Excellent edge retention. Specifically for plasma transferred arc (PTA) application.

Information provided by Wall Colmonoy Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 11.78 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 43 - 48single pass
 50 - 55double pass
 
Thermal PropertiesOriginal ValueComments
Melting Point 2040 °F
 
Component Elements PropertiesOriginal ValueComments
Boron, B 0.90 %
Carbon, C 2.0 %
Chromium, Cr 20.3 %
Iron, Fe 1.4 %
Nickel, Ni 40 %As Balance
Silicon, Si 1.4 %
Tungsten, W 34 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Wall Colmonoy COLMONOY® 56 Hard-Surfacing Alloy Containing Wear-Resistant Chromium Borides and Carbides
Wall Colmonoy COLMONOY® 57 PTA Nickel-Base Hard-Surfacing Alloy
Wall Colmonoy COLMONOY® 56 PTA Nickel-Base Hard-Surfacing Alloy With Chromium Boride
Wall Colmonoy COLMONOY® 88 Hard-Surfacing Alloy
Wall Colmonoy COLMONOY® 5 PTA Nickel-Base Hard Surfacing Alloy With Chromium Boride

NWALL19 / 19786

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.