MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Mafic Assembled Basalt Roving 300 to 2000 Tex
Categories: Ceramic; Other Engineering Material; Composite Fibers

Material Notes: Continuous filaments produced from basalt rock used for reinforcement of thermoplastics and thermosets.

Single-end Assembled Roving or Multi-end Assembled Roving available. Internal and External Payout available. Sizing available (sizing agent = silane) for polypropylene, epoxy, vinyl ester, polyester, polyurethane, nylon, or PET/PBT. Also available unsized with deionized water only as the sizing agent.

Information provided by Mafic Basalt

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.63 g/cc0.0950 lb/in³DIN 65569
Loss On Ignition >= 0.40 %>= 0.40 %Varies with Sizing
Filament Diameter 13 - 19 µm13 - 19 µmMay be specified
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 3100 MPa450000 psiASTM D2343
Elongation at Break 3.5 %3.5 %
Tensile Modulus 88.0 - 92.0 GPa12800 - 13300 ksiASTM D2343
Tenacity >= 0.650 N/tex>= 7.36 g/denier
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.10 %<= 0.10 %
 
Descriptive Properties
Linear Density300-2000 Tex(+/-5%)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Beijing Evergrow Resources BF-6 Basalt Needle Felt
Beijing Evergrow Resources BF-3 Basalt Needle Felt
A-Glass Fiber, Generic
Mafic Chopped Basalt Fiber for Concrete
SGL Carbon Group PANOX® LB C076 SSC Oxidized Textile Fiber, Crimped staple fiber, For felts and non-wovens

EMAFC001 / 187062

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.