MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

ChevronTexaco ECO® SAE 40 Heavy Duty Motor Oil
Categories: Fluid; Lubricant

Material Notes: Features:

Chevron ECO Heavy Duty Motor Oils are formulated to be environmentally responsible engine lubricants.

They use the highest quality re-refined base oils and specially selected additives designed to provide excellent performance in all recommended applications.

They contain an effective detergent dispersant to keep sulfated ash to a minimum. They are fortified with oxidation and corrosion inhibitors, high temperature antiwear additives, and foam inhibitors to protect vital engine parts from scuffing and protect the bearings from corrosion.

Chevron ECO Heavy Duty Motor Oil SAE 15W-40 is designed to meet the warranty requirements of most manufacturers of diesel engines. The high alkaline reserve (base number) effectively protects bearings and other engine surfaces from the corrosive effect of acids formed by the combustion of high sulfur fuels.

Applications

Chevron ECO Heavy Duty Motor Oils:

  • exceed the requirements of Caterpillar Series 3 and are recommended when the sulfur content of the fuel is unknown or exceeds 0.50%.
  • exceed the Mack EO K/2 specification. Mack’s preferred recommendation is SAE 15W-40.
  • meet and exceed service requirements for Cummins and Detroit Diesel engines when recommending these viscosity grades.
  • are recommended for all turbocharged engines where the manufacturer specified a Caterpillar Series 3 oil.
  • are not recommended for Electro Motive Diesel engines with silver bearings.
  • can also be used in gasoline passenger cars and light trucks.

Key Words: CPS Number: 222430; MSDS Number: 7558
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
API Gravity 27.7 °27.7 °
Viscosity Measurement 105105Viscosity Index; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 159.7 cSt159.7 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 16.1 cSt16.1 cStASTM D445
Ash 1.2 %1.2 %Sulfated Ash wt%
 
Chemical PropertiesMetricEnglishComments
Total Base Number 8.08.0ASTM D2896
 
Thermal PropertiesMetricEnglishComments
Pour Point -15.0 °C5.00 °FASTM D97
Flash Point 238 °C460 °FASTM D92
 
Component Elements PropertiesMetricEnglishComments
Phosphorus, P 0.10 %0.10 %
Zinc, Zn 0.11 %0.11 %
 
Descriptive Properties
Re-refined Oil Content, % of Base Oil100

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WCHEV017 / 74632

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.