MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
LATI Latilon 28D PC
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: Polycarbonate (PC). Unfilled. Low smoke density and low toxicity index. Very high dimensional stability. Very good surface appearance

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Information provided by Lati Industria Termoplastici S.p.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/cc
Linear Mold Shrinkage, Flow 0.0070 - 0.0090 cm/cm
Linear Mold Shrinkage, Transverse 0.0070 - 0.0090 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Elongation at Break >= 100 %
@Temperature 23.0 °C
 >= 100 %
@Temperature 60.0 °C
 >= 100 %
@Temperature 90.0 °C
 >= 100 %
@Temperature 120 °C
Elongation at Yield 2.5 %
@Temperature 120 °C
 3.5 %
@Temperature 90.0 °C
 4.5 %
@Temperature 60.0 °C
 6.0 %
@Temperature 23.0 °C
Tensile Modulus 1600 MPa
@Temperature 120 °C
 1800 MPa
@Temperature 90.0 °C
 2100 MPa
@Temperature 60.0 °C
 2400 MPa
@Temperature 23.0 °C
Charpy Impact Unnotched NB
@Temperature 23.0 °C
 NB
@Temperature -20.0 °C
Charpy Impact, Notched 8.00 kJ/m²
@Temperature -20.0 °C
 10.0 kJ/m²
@Temperature 23.0 °C
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 120 °C
Deflection Temperature at 0.46 MPa (66 psi) 125 °C
Deflection Temperature at 1.8 MPa (264 psi) 120 °C
Vicat Softening Point 135 °C
@Load 5.00 kg
Oxygen Index 26 %
 
Processing PropertiesOriginal ValueComments
Melt Temperature 270 - 290 °C
Mold Temperature 100 - 120 °C
Drying Temperature 120 - 130 °C
@Time 10800 sec
 
Descriptive Properties
ISO Shrinkage - Pressure60 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient LubriOne™ PC-000/15T Polycarbonate (PC)
Covestro Makrolon® 6357 Polycarbonate, Flame Retardant Grade
Celanese FORTRON 205 PPS, Unfilled
Teijin Panlite® LN-2250Z Polycarbonate
Overview of materials for Polyphenylene Sulfide (PPS); Molded

PLATH9842 / 177538

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.