MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Fujipoly Industries Sarcon® NR-c Gap Filler Pad Non-Silicone
Categories: Polymer

Material Notes: Sarcon NR-c consists of an Acrylate resin and some thermal conductive fillers. It is a highly conformable/ thermally conductive material in a versatile sheet form that makes reliable and complete physical contact. Not electrically conductive

Information provided by Fujipoly Industries

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.10 g/cc2.10 g/cc-40°C for 1,000 hrs; JIS-K-6220; ASTM D 792
 2.10 g/cc2.10 g/cc-40°C for 30 min and 125°C for 30 min. for 1,000 times; JIS-K-6220; ASTM D 792
 2.10 g/cc2.10 g/cc80°C for 1,000 hrs; JIS-K-6220; ASTM D 792
 2.10 g/cc2.10 g/cc85°C for 1,000 hrs with 85% RH; JIS-K-6220; ASTM D 792
 2.10 g/cc2.10 g/ccJIS-K-6220; ASTM D-792
 2.20 g/cc2.20 g/cc125°C for 1,000 hrs; JIS-K-6220; ASTM D 792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore C 282885°C for 1,000 hrs with 85% RH; SRIS0101S
 3030-40°C for 1,000 hrs; SRIS0101S
 303080°C for 1,000 hrs; SRIS0101S
 3737-40°C for 30 min and 125°C for 30 min. for 1,000 times; SRIS0101S
 5555125°C for 1,000 hrs; SRIS0101S
Hardness, Shore OO 5353ASTM D-2240
Tensile Strength, Yield 0.200 MPa29.0 psi85°C for 1,000 hrs with 85% RH; JIS-K-6251(#2); ASTM D412
 0.200 MPa29.0 psi-40°C for 1,000 hrs; JIS-K-6251(#2); ASTM D412
 0.200 MPa29.0 psiJIS-K-6251(#2)/ASTM D-412
 0.300 MPa43.5 psi80°C for 1,000 hrs; JIS-K-6251(#2); ASTM D412
 0.800 MPa116 psi125°C for 1,000 hrs; JIS-K-6251(#2); ASTM D412
 0.800 MPa116 psi-40°C for 30 min and 125°C for 30 min. for 1,000 times; JIS-K-6251(#2); ASTM D412
Elongation at Yield 20 %20 %125°C for 1,000 hrs; JIS-K-6251(#2); ASTM D412
 25 %25 %-40°C for 30 min and 125°C for 30 min. for 1,000 times; JIS-K-6251(#2); ASTM D412
 150 %150 %JIS-K-6251(#2)/ASTM D-412
 180 %180 %80°C for 1,000 hrs; JIS-K-6251(#2); ASTM D412
 180 %180 %85°C for 1,000 hrs with 85% RH; JIS-K-6251(#2); ASTM D412
 180 %180 %-40°C for 1,000 hrs; JIS-K-6251(#2); ASTM D412
Tear Strength 1.50 kN/m8.56 pliJIS-K-6252 (Angle)/ASTM D-624
 1.70 kN/m9.70 pli-40°C for 1,000 hrs; JIS-K-6252(Angle); ASTM D624
 1.80 kN/m10.3 pli80°C for 1,000 hrs; JIS-K-6252(Angle)/ASTM D 624
 2.00 kN/m11.4 pli85°C for 1,000 hrs with 85% RH; JIS-K-6252(Angle); ASTM D 624
 5.70 kN/m32.5 pli-40°C for 30 min and 125°C for 30 min. for 1,000 times; JIS-K-6252(Angle); ASTM D 624
 7.40 kN/m42.2 pli125°C for 1,000 hrs; JIS-K-6252 (Angle); ASTM D 624
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 7.00e+6 ohm-cm7.00e+6 ohm-cm-40°C for 1,000 hrs; JIS-K-6249; ASTM D257
 2.00e+11 ohm-cm2.00e+11 ohm-cmJIS-K-6249/ASTM D257
 8.00e+11 ohm-cm8.00e+11 ohm-cm85°C for 1,000 hrs with 85% RH; JIS-K 6249; ASTM D257
 1.00e+12 ohm-cm1.00e+12 ohm-cm-40°C for 30 min and 125°C for 30 min. for 1,000 times; JIS-K-6249; ASTM D149
 2.00e+12 ohm-cm2.00e+12 ohm-cm80°C for 1,000 hrs; JIS-K-6249; ASTM D 257
 3.00e+13 ohm-cm3.00e+13 ohm-cm125°C for 1,000 hrs; JIS-K-6249; ASTM D257
Dielectric Strength 9.00 kV/mm229 kV/in-40°C for 1,000 hrs; JIS-K-6249; ASTM D149
 11.0 kV/mm279 kV/inJIS-K-6249; ASTM D-149
 18.0 kV/mm457 kV/in80°C for 1,000 hrs; JIS-K-6249; ASTM D 149
 26.0 kV/mm660 kV/in125°C for 1,000 hrs; JIS-K-6249; ASTM D 149
 27.0 kV/mm686 kV/in-40°C for 30 min and 125°C for 30 min. for 1,000 times; JIS-K-6249; ASTM D 149
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 1.50 W/m-K10.4 BTU-in/hr-ft²-°FJIS-R-2618; ASTM D2326
Maximum Service Temperature, Air 105 °C221 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
Flammability, UL94 V-0V-0
 
Descriptive Properties
ColorGrey

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow Appeel® 20D784 Ethylene Acrylate
Fujipoly Industries Sarcon® NR-HTc Gap Filler Pad
Dow Appeel® LSR20D751 Lidding Sealant Resin
Park Aerospace Nelcote® V-341 Polybutadiene Prepreg, 120 E-Glass Reinforced
Dow Appeel® 22D843 Ethylene Acrylate

PFUJIP58 / 39191

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.