MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Unifrax Fiberfrax® Duraboard® HD Ceramic Fiber Board
Categories: Ceramic; Oxide; Aluminum Oxide; Silicon Oxide

Material Notes: Fiberfrax® Duraboard® products are a family of rigid, high-temperature ceramic fiber boards manufactured in a wet forming process using Fiberfrax alumina-silica fibers and binders. All Duraboard products offer low thermal conductivity, high temperature stability, uniform density, and excellent resistance to thermal shock and chemical attack.

Duraboard HD insulation is a high-density board product that offers the same high level of dimensional and surface uniformity as Duraboard LD insulation, but provides enhanced compressive strength and a higher modulus of rupture. This higher density is achieved through the inclusion of clay additives during the manufacturing process. Its higher strength makes Duraboard HD insulation particularly well-suited to weight load support applications such as refractory brick backup or for covering larger unsupported spans.

Description: The addition of clay gives a higher density, MOR, and strength.

Information Provided by Unifrax I LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.417 g/cc0.0150 lb/in³Nominal
Loss On Ignition 6.0 - 7.0 %6.0 - 7.0 %
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture 0.000862 GPa0.125 ksiFired (24 hrs at cont. use)
 0.00207 GPa0.300 ksiGreen (typ.)
Compressive Strength 0.221 MPa32.0 psi15% Deformation; Fired
 0.228 MPa33.0 psi10% Deformation; Fired
 0.241 MPa35.0 psi5% Deformation; Fired
 0.407 MPa59.0 psi5% Deformation; Green
 0.483 MPa70.0 psi10% Deformation; Green
 0.558 MPa81.0 psi15% Deformation; Green
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 1.06 kV/mm27.0 kV/in
 
Thermal PropertiesMetricEnglishComments
Melting Point 1760 °C3200 °F
Maximum Service Temperature, Air 1149 °C2100 °FRecommended Operating Temperature
Shrinkage <= 5.0 %
@Time 86400 sec
<= 5.0 %
@Time 24.0 hour
at Recommended Operating Temperature
 
Descriptive Properties
ColorCream
Fiberfrax® Fibers (%)100
Temperature Grade (°C)1260

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Unifrax Fiberfrax® Fibermat® Blanket Ceramic Fiber Insulator
Unifrax Fiberfrax® Durablanket® 2600 Ceramic Fiber Insulator
Unifrax Fiberfrax® Durablanket® S Ceramic Fiber Insulator
Unifrax Fiberfrax® Fibermax® Mat Ceramic Fiber Insulator
Unifrax Fiberfrax® Durablanket® HP-S Ceramic Fiber Insulator

CUNIF028 / 97800

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.