MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Phillips 66 Kendall® Non-Detergent Motor Oil SAE Grade 30
Categories: Fluid; Lubricant

Material Notes: Kendall® Non-Detergent Motor Oil is a high-quality, non-detergent engine oil recommended primarily for use in industrial applications where a non-detergent oil is specified. The SAE 30 viscosity grade also may be used in gasoline engines operated under such mild conditions that higher quality compounded oils are not required. It meets former API Service SB performance requirements. Non-Detergent Motor Oil is formulated to provide good wear protection and resistance to oxidation, rust, corrosion and foaming.

Applications:

  • Air compressors and other industrial applications where a non-detergent oil is specified
  • Gasoline engines operated under such mild conditions that compounded oils are not required
Non-Detergent Motor Oil meets the requirements of:
  • API Service SB
Features/Benefits:
  • Good oxidation resistance
  • Protects against wear
  • Protects against rust and corrosion
  • Good foam resistance

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.878 g/cc0.878 g/cc
Density 0.877 g/cc0.0317 lb/in³
Viscosity Measurement 104104Index
Saybolt Viscosity at 100°F 478 SUS478 SUS
Saybolt Viscosity at 210°F 63.9 SUS63.9 SUS
Kinematic Viscosity at 40°C (104°F) 92 cSt92 cSt
Kinematic Viscosity at 100°C (212°F) 11 cSt11 cSt
Ash <= 0.10 %<= 0.10 %Sulfated; ASTM D874
ASTM Color 0.500.50ASTM D1500
 
Thermal PropertiesMetricEnglishComments
Pour Point -15.0 °C5.00 °F
Flash Point 240 °C464 °FCOC
 
Component Elements PropertiesMetricEnglishComments
Phosphorus, P 0.050 %0.050 %
Zinc, Zn 0.060 %0.060 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WCON6473 / 210044

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.