MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Vibrantz Technologies CS 713 Metal Sealing
Categories: Ceramic; Glass

Material Notes: Glass Type: Si-Ba Alkali
Typical Powder Form: VSD
Typical Application: Compress.

Ferro Metal Sealing glasses are formulated for sealing a wide range of metal packages and parts, including matched seals for Kovar, molybdenum, nickel, copper, and aluminum; and compression seals for stainless steel and iron with alloy pins. These products are available in VSD mesh powder as well as custom milled forms suitable for granulation for use in pressing operations.

Information provided by Ferro Corporation

Ferro Corporation is now a part of Vibrantz Technologies.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.65 g/cc
Particle Mesh Size 200 Mesh
 
Thermal PropertiesOriginal ValueComments
CTE, linear 9.30 µm/m-°Cat Set Pt.
 8.80 µm/m-°C
@Temperature 260 °C
Softening Point 655 °C
Annealing Point 515 °C
Transformation Temperature 485 °C
 
Processing PropertiesOriginal ValueComments
Processing Temperature 950 °CTypical Firing Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

CFERR39 / 853

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.