MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Wacker Semicosil® 989/1K Silicone Adhesive
Categories: Polymer; Thermoset; Silicone

Material Notes: SEMICOSIL® 989/1K is a non-slump, thermally curable, addition curing one-part silicone rubber.

Special features:

  • one-part, ready-to-use
  • thixotropic
  • transparent
  • medium hardness
  • high flexibility (low-stress-adhesive)
  • rapid heat curing
  • primerless adhesion to many substrates
Application:
    general purpose adhesive for the electronics industry
  • FIPG and CIPG applications

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.10 g/cc0.0397 lb/in³cured; ISO 2781
 1.10 g/cc0.0397 lb/in³uncured; DIN 53479
Viscosity  30000 cP
@Shear Rate 25.0 1/s
30000 cP
@Shear Rate 25.0 1/s
cured; ISO 3219
 300000 cP
@Shear Rate 0.500 1/s
300000 cP
@Shear Rate 0.500 1/s
uncured; ISO 3219
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5555ISO 868
Tensile Strength at Break 5.00 MPa725 psiISO 37
Elongation at Break 200 %200 %ISO 37
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %cured. "Transparent" but manufacturer does not quantify.
 90 %90 %uncured. "Transparent" but manufacturer does not quantify.
 
Processing PropertiesMetricEnglishComments
Cure Time  60.0 min
@Treatment Temp. 130 °C
1.00 hour
@Treatment Temp. 266 °F
in a circuatling air oven
 360 min
@Treatment Temp. 100 °C
6.00 hour
@Treatment Temp. 212 °F
 
Descriptive Properties
Colortransparentcured
 transparentuncured

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Wacker Semicosil® 936 UV Conformal Coating

PWACK9428 / 204957

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.