MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Akoalit PB 4268 white Polyolefin
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: Akoalit polybutene-1 homopolymers (PB-H) show improved water quality properties providing the potential to meet stringent future organoleptic requirements. An increased melt flow ratio (MFR) allows up to 50% faster processing due to reduced sensitivity to process-induced orientation. Akoalit PB 4268 white is a premium highly isotactic homo polyolefin manufactured from butene-1 monomer. The product provides excellent long term hydrostatic strength also at elevated temperatures combined with high flexibility. Akoalit PB 4268 complies with requirements specified in ISO 15876, ISO 12230, DIN 16968/DIN 16969 and many other National Standards for PB-1 pipe applications. The grade is typically used for high-performance extrusion into pipe and injection molding into fittings for potable hot and cold water distribution applications where improved organoleptic properties are required. Akoalit PB 4268 is available in white color in pellet form. Akoalit PB 4268 may not be used in the manufacture of pipe applications intended for sale or shipment to North America, without prior written approval by manufacturer for each specific product and application.

Applications: District Heating, Drinking Water Pipe, Industrial, Radiator Connections, Underfloor Heating.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.925 g/ccISO 1183-1
Melt Flow 0.60 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133-1
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 30.0 MPaISO 8986-2
Tensile Strength, Yield 17.0 MPaISO 8986-2
Elongation at Break 225 %ISO 8986-2
Flexural Modulus 450 MPaISO 178
 
Processing PropertiesOriginal ValueComments
Processing Temperature 180 - 200 °CExtrusion Temperature
 200 - 240 °CInjection Molding Temperature
 
Descriptive Properties
Cooling Water Temperature (°C)10 to 12
Processing MethodPipe, Sheet
Vacuum (mbar)30 to 60

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Carmel Olefins Capilene® G 65 F Polypropylene Homopolymer
Borealis Borclean™ HB311BF Polypropylene Homopolymer for Capacitor Film
LyondellBasell Akoalit PB 4267 Grey Polyolefin
LyondellBasell Adstif HA 716J Polypropylene
LyondellBasell Adstif HA 3105 Polypropylene

PEQT7055 / 218693

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.