MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Caplinq LINQSTAT™ VCF-41014B
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: Product Description: LINQSTAT™ VCF-Series is a black, carbon-filled, volume-conductive polyethylene film designed to provide both physical and static protection in numerous semiconductor, electronic, and Smartcard applications. Its easy-grounding nature makes it ideal for packaging where electrostatic contamination is a problem. The film and its conductivity are unaffected by humidity and age. The film is heat-sealable, flexible and offers exceptional abrasion resistance. Additionally, the film gives good thermal stability and has outstanding chemical resistance. The conductive bags meet electrical requirements of the military specification MIL-P-82646.

Applications:

  • Protection and storage of static-sensitive components
  • Interleaf between rolls of Smartcard modules
  • Grounding Mats

Product Features and Benefits:

  • Volume-conductive plastic
  • Black Opaque - Printable
  • Provides anti-static protection to electronic components
  • Groundable
  • Humidity indepentent conductivity

Chemical Susceptibility

  • Methanol: Resistant
  • Ethanol: Resistant
  • Isopropanol: Resistant
  • Weak Acids: Resistant
  • Ketones (Acetone): Slow Attack
  • Weak Alkalines: Slow Attack
  • Hydrocarbons: Non-Resistant

Information provided by Caplinq

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 65.0 - 200 microns
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 13.8 MPaASTM-D882
Film Elongation at Break, MD 330 %ASTM-D882
Film Elongation at Break, TD 390 %ASTM-D882
Dart Drop Test 380 - 400 g50% Failure Weight; ASTM D1709-67
Heat Seal Strength 3.00 - 9.23 g/25 mmTransverse Direction; ASTM-D882
 3.51 - 10.8 g/25 mmMachine Direction; ASTM-D882
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity <= 500 ohm-cmASTM-D991
Surface Resistivity per Square <= 31000 ohmMIL 81705C
Static Decay <= 2.0 secEIA - Std 541

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Alliance Polymers Zythane™ 4080A Thermoplastic Polyurethane Elastomer
Alliance Polymers Zythane™ 4060A Thermoplastic Polyurethane Elastomer
3D Systems DuraForm® TPU Elastomer Thermoplastic Elastomer for SLS® Systems
SK Chemicals SKYTHANE® 190A S series Polyurethane
ExxonMobil Santoprene® 8201-80HT Thermoplastic Elastomer

PCAPL014 / 90287

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.