MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Magnesium
Magnesium Elektron - Service & Innovation in Magnesium

(Viewing data as-entered. Click here to return)
Magnesium Elektron Elektron® AZ31B Magnesium Extrusion Alloy, UNS M11311
Categories: Metal; Nonferrous Metal; Magnesium Alloy

Material Notes: AZ31B is a wrought magnesium base alloy with good room-temperature strength and ductility combined with corrosion resistance and weldability. Increased strength is obtained by strain hardening with a subsequent partial anneal (H24 and H26 tempers).

Applications: Sheet and plate in AZ31B find application in medium strength service at temperatures below 150°C. Diverse uses including aircraft fuselage, concrete tools, cell phone/camera/notebook computer cases, speaker cones and textile machinery can all benefit from light weight AZ31B. AZ31B is non-magnetic and has high electrical and thermal conductivity filling the requirements for RFI and EMI shielding in the electronics and computer industries. Superplastic forming of AZ31B sheet at elevated temperatures allows production of a wide variety of intricate parts for automotive uses. Monocoque construction utilizing formed sheet can be adapted to many commercial applications.

Information provided by Magnesium Elektron.

Key Words: UNS M11311; AMS 4375; AMS 4376; AMS 4377; AMS 4382; ASTM B90
Vendors: Magnesium Elektron is the world leader in high strength magnesium alloys in rolled, extruded and cast forms. Phone (303) 589-3189 or visit www.magnesium-elektron.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.78 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell E 67O temper
 83H24 temper
Tensile Strength at Break 30.0 MPa
@Temperature 300 °C
 95.0 MPa
@Temperature 200 °C
 200 MPa
@Temperature 100 °C
 220 MPa
@Thickness 0.500 - 1.50 mm
AZ31B-O
 220 MPa
@Thickness 1.50 - 6.30 mm
AZ31B-O
 220 MPa
@Thickness 6.30 - 7.50 mm
AZ31B-O
 235 MPa
@Thickness 25.0 - 50.0 mm
AZ31B-H24
 235 MPa
@Thickness 50.0 - 75.0 mm
AZ31B-H24
 240 MPa
@Thickness 25.0 - 50.0 mm
AZ31B-H26
 245 MPa
@Thickness 12.7 - 25.0 mm
AZ31B-H24
 255 MPa
@Thickness 9.50 - 12.7 mm
AZ31B-H24
 255 MPa
@Thickness 12.7 - 25.0 mm
AZ31B-H26
 255 MPa
@Thickness 25.0 - 75.0 mm
 260 MPa
@Thickness 6.30 - 12.7 mm
AZ31B-H26
 260 MPa
@Thickness 6.30 - 9.50 mm
AZ31B-H24
 265 MPa
@Thickness 10.0 - 25.0 mm
 270 MPa
@Thickness 0.500 - 6.30 mm
AZ31B-H24
 275 MPa
@Thickness 5.00 - 10.0 mm
 290 MPa
@Thickness 0.500 - 6.00 mm
Tensile Strength, Yield 25.0 MPa
@Strain 0.2 %,
Temperature 300 °C
 50.0 MPa
@Strain 0.2 %,
Temperature 200 °C
 150 MPa
@Strain 0.2 %,
Temperature 100 °C
 105 MPa
@Strain 0.2 %,
Thickness 1.50 - 6.30 mm
AZ31B-O
 105 MPa
@Strain 0.2 %,
Thickness 6.30 - 7.50 mm
AZ31B-O
 125 MPa
@Strain 0.2 %,
Thickness 50.0 - 75.0 mm
AZ31B-H24
 125 MPa
@Strain 0.2 %,
Thickness 0.500 - 1.50 mm
AZ31B-O
 135 MPa
@Strain 0.2 %,
Thickness 25.0 - 50.0 mm
AZ31B-H24
 145 MPa
@Strain 0.2 %,
Thickness 25.0 - 50.0 mm
AZ31B-H26
 150 MPa
@Strain 0.2 %,
Thickness 25.0 - 75.0 mm
 150 MPa
@Strain 0.2 %,
Thickness 12.7 - 25.0 mm
AZ31B-H24
 160 MPa
@Strain 0.2 %,
Thickness 12.7 - 25.0 mm
AZ31B-H26
 165 MPa
@Strain 0.2 %,
Thickness 9.50 - 12.7 mm
AZ31B-H24
 175 MPa
@Strain 0.2 %,
Thickness 10.0 - 25.0 mm
 180 MPa
@Strain 0.2 %,
Thickness 6.30 - 12.7 mm
AZ31B-H26
 180 MPa
@Strain 0.2 %,
Thickness 6.30 - 9.50 mm
AZ31B-H24
 200 MPa
@Strain 0.2 %,
Thickness 0.500 - 6.30 mm
AZ31B-H24
 200 MPa
@Strain 0.2 %,
Thickness 6.00 - 10.0 mm
 220 MPa
@Strain 0.2 %,
Thickness 0.500 - 6.00 mm
Elongation at Break 35 %
@Temperature 100 °C
 85 %
@Temperature 200 °C
 135 %
@Temperature 300 °C
 5.0 %
@Thickness 6.30 - 12.7 mm
AZ31B-H26
 5.0 %
@Thickness 12.7 - 25.0 mm
AZ31B-H26
 5.0 %
@Thickness 25.0 - 50.0 mm
AZ31B-H26
 5.0 %
@Thickness 0.500 - 6.30 mm
AZ31B-H24
 7.0 %
@Thickness 6.30 - 9.50 mm
AZ31B-H24
 7.0 %
@Thickness 9.50 - 12.7 mm
AZ31B-H24
 7.0 %
@Thickness 12.7 - 25.0 mm
AZ31B-H24
 7.0 %
@Thickness 25.0 - 50.0 mm
AZ31B-H24
 7.0 %
@Thickness 50.0 - 75.0 mm
AZ31B-H24
 8.0 %
@Thickness 6.30 - 7.50 mm
AZ31B-O
 10 %
@Thickness 0.500 - 1.50 mm
AZ31B-O
 10 %
@Thickness 1.50 - 6.30 mm
AZ31B-O
 13 %
@Thickness 0.500 - 6.00 mm,
Temperature 22.0 °C
 13 %
@Thickness 25.0 - 75.0 mm,
Temperature 22.0 °C
 15 %
@Thickness 5.00 - 10.0 mm,
Temperature 22.0 °C
 16 %
@Thickness 10.0 - 25.0 mm,
Temperature 22.0 °C
Creep Strength 10.0 MPa
@Temperature 150 °C,
Time 360000 sec
0.1% creep
 20.0 MPa
@Temperature 150 °C,
Time 36000 sec
0.1% creep
 25.0 MPa
@Temperature 150 °C,
Time 360000 sec
0.2% creep
 30.0 MPa
@Temperature 100 °C,
Time 360000 sec
0.1% creep
 35.0 MPa
@Temperature 100 °C,
Time 36000 sec
0.1% creep
 35.0 MPa
@Temperature 150 °C,
Time 36000 sec
0.2% creep
 40.0 MPa
@Temperature 150 °C,
Time 360000 sec
0.5% creep
 50.0 MPa
@Temperature 150 °C,
Time 36000 sec
0.5% creep
 50.0 MPa
@Temperature 100 °C,
Time 360000 sec
0.2% creep
 60.0 MPa
@Temperature 100 °C,
Time 36000 sec
0.2% creep
 85.0 MPa
@Temperature 100 °C,
Time 360000 sec
0.5% creep
 95.0 MPa
@Temperature 100 °C,
Time 36000 sec
0.5% creep
 102 MPa
@Temperature 100 °C,
Time 360000 sec
1% creep
 110 MPa
@Temperature 100 °C,
Time 36000 sec
1% creep
Modulus of Elasticity 45.0 GPa
Compressive Yield Strength 85.0 MPa
@Strain 0.2 %,
Thickness 50.0 - 75.0 mm
 95.0 MPa
@Strain 0.2 %,
Thickness 25.0 - 50.0 mm
 120 MPa
@Strain 0.2 %,
Thickness 10.0 - 25.0 mm
 160 MPa
@Strain 0.2 %,
Thickness 6.00 - 10.0 mm
 180 MPa
@Strain 0.2 %,
Thickness 0.500 - 6.00 mm
Poissons Ratio 0.35
Fatigue Strength 110 MPa
@# of Cycles 1.00e+7
Cantilever bending
 125 MPa
@# of Cycles 1.00e+6
Cantilever bending
 150 MPa
@# of Cycles 100000
Cantilever bending
Fracture Toughness 28.0 MPa-m½KIC
Shear Strength 180 MPa
@Thickness 10.0 - 75.0 mm
 195 MPa
@Thickness 6.00 - 10.0 mm
 200 MPa
@Thickness 0.500 - 6.00 mm
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000920 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 26.8 µm/m-°C
Specific Heat Capacity 1.04 J/g-°C
Thermal Conductivity 76.9 W/m-K
Melting Point 566 - 632 °C
Solidus 566 °C
Liquidus 632 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 2.5 - 3.5 %
Magnesium, Mg 94.2 - 96.6 %As Balance
Manganese, Mn 0.20 - 1.0 %
Zinc, Zn 0.70 - 1.3 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Magnesium Elektron Elektron® 21 Magnesium Casting Alloy
Overview of materials for Magnesium Alloy
Magnesium, Mg; Annealed Sheet
Magnesium, Mg; Hard-Rolled Sheet
Magnesium Elektron Elektron® AZ91 Magnesium Alloy

NMAGEL938 / 186953

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.