MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Polymer Resources AC-GP2 Acetal Copolymer, Medium Flow  (discontinued **)
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Unreinforced

Material Notes: Process: Molding or Extrusion
Notes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.

Information provided by Polymer Resources Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.41 g/cc1.41 g/ccASTM D792
Linear Mold Shrinkage 0.018 - 0.022 cm/cm0.018 - 0.022 in/inASTM D955
Melt Flow 6.0 - 12 g/10 min
@Load 2.16 kg,
Temperature 190 °C
6.0 - 12 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 61.4 MPa8900 psiASTM D638
Tensile Strength, Yield 61.4 MPa8900 psiASTM D638
Flexural Strength 90.3 MPa13100 psiASTM D790
Flexural Modulus 2.60 GPa377 ksiASTM D790
Izod Impact, Notched 0.641 J/cm
@Temperature 22.8 °C
1.20 ft-lb/in
@Temperature 73.0 °F
ASTM D256
Gardner Impact 22.6 J16.7 ft-lbASTM D3029
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 157 °C315 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 110 °C230 °FASTM D648
Flammability, UL94  HB
@Thickness 1.59 mm
HB
@Thickness 0.0626 in
 HB
@Thickness 3.17 mm
HB
@Thickness 0.125 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 168 - 174 °C335 - 345 °F
Middle Barrel Temperature 179 - 185 °C355 - 365 °F
Front Barrel Temperature 185 - 191 °C365 - 375 °F
Melt Temperature 182 - 199 °C360 - 390 °F
Mold Temperature 76.7 - 93.3 °C170 - 200 °F
Drying Temperature 79.4 - 85.0 °C175 - 185 °F
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hour
Vent Depth 0.00127 cm0.000500 in

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
VICTREX™ PEEK 450G™ General Purpose
INEOS Styrolution Terluran® GP-22 ABS
Dow HDPE 17450N High Density Polyethylene
Dow H7012-35RN Polypropylene Homopolymer Resin
Delrin Delrin® 500P BK602 POM

PPOLYQ016 / 160530

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.