MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Shanghai Potomer 1010 Phenolic Antioxidant
Categories: Other Engineering Material

Material Notes: CAS NO. 6683-19-8

Introduction: Phenolic Antioxidant 1010 is white powder, has not scented tastelessly. Nature is steady. It is apt to dissolve it in such solvents as the benzene, acetone and ester, etc, do not dissolve in water, dissolve in the ethanol a little. It is fine that this product is pollution-free, heat resisting and is able to bear water taking out, compatibility is good.

Applications: Phenolic Antioxidant 1010 is that a kind of pluralism is obstructed the phenol type and resisted oxygen pharmaceutical, have very good compatibility with most polymer. There is good function of changing color of preventing the light and heat from causing. Used PE, PP, PS, polyamide, polyformaldehyde, ABS resin, PVC, synthetic rubber, etc. in the high polymer material extensively. Used for preventing the hot oxygen of the oil and coating from wearing out too.

Information provided by Shanghai Potomer International Trade Co., Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles <= 0.50 %<= 0.50 %
Ash <= 0.10 %<= 0.10 %
 
Thermal PropertiesMetricEnglishComments
Melting Point 110 - 125 °C230 - 257 °F
 
Optical PropertiesMetricEnglishComments
Transmission, Visible  >= 93 %
@Wavelength 425 nm
>= 93 %
@Wavelength 425 nm
 >= 95 %
@Wavelength 500 nm
>= 95 %
@Wavelength 500 nm
 
Descriptive Properties
Color/AppearanceWhite powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSPOTOM135 / 284581

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.