MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Multibase Multi-ABS 3245 FR Flame Retardant ABS
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant

Material Notes: Data provided by Multibase.

Key Words: Poly(Acrylonitrile Butadiene Styrene)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.23 g/cc0.0444 lb/in³ASTM D792-91
Linear Mold Shrinkage 0.0050 cm/cm0.0050 in/inASTM D955-89
Melt Flow 5.0 g/10 min5.0 g/10 min(Condition G) ASTM D-1238-94a
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 38.6 MPa5600 psiASTM D638-95
Elongation at Break 40 %40 %ASTM D638-95
Flexural Modulus 2.241 GPa325.0 ksiRT; ASTM D-790-95
Izod Impact, Notched 2.14 J/cm4.01 ft-lb/inASTM D256-93a
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 165 °C329 °Finjection molded unannealed; ASTM D-648-95
 185 °C365 °Finjection molded annealed; ASTM D-648-95
 195 °C383 °Fcompression molded annealed; ASTM D-648-95
Vicat Softening Point 99.0 °C210 °FASTM D1525-95
Flammability, UL94  V-0
@Thickness 1.59 mm
V-0
@Thickness 0.0625 in
UL 94
 V-0
@Thickness 3.17 mm
V-0
@Thickness 0.125 in
UL 94
 
Optical PropertiesMetricEnglishComments
Gloss 55 %55 %ASTM D2457-90

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Westlake Plastics Lennite® GUR1050 (Type II) UHMW-PE For Medical Applications
Westlake Plastics Lennite® GUR1020 (Type I) UHMW-PE For Medical Applications
Multibase Multi-ABS 802 Natural Extrusion Grade
Multibase Multi-ABS 801 Natural Extrusion Grade
Multibase Multi-ABS 3845 Medium Impact ABS

PLA292 / 49689

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.