MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Skamol Group Skamol FL-06 Insulating Mortar
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: SKAMOL insulating mortars have the following characteristics:
  • Max. service temperature: Up to 1150°C (2102°F)
  • Dry-mix mortars designed for use with Skamol insulating bricks/blocks and slab grades in various applications
  • Good insulation values
  • Outstanding bonding properties within max. service temperature range
  • Water-retentive properties for quick and easy laying of dry bricks/blocks/slabs.
  • Combined air and heat-setting.

Information provided by Skamol.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 1.30 g/cc0.0469 lb/in³As Supplied
 1.60 g/cc0.0579 lb/in³Dried at 110°C (230°F)
Loss On Ignition 4.1 %
@Temperature 1025 °C
4.1 %
@Temperature 1877 °F
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 1150 °C2100 °F
 
Component Elements PropertiesMetricEnglishComments
Al2O3 40 %40 %
CaO 0.40 %0.40 %
Fe2O3 1.2 %1.2 %
H2O, Water 2.0 %2.0 %as supplied
K2O 1.6 %1.6 %
MgO 0.90 %0.90 %
Na2O 3.6 %3.6 %
SiO2 46 %46 %
TiO2 1.5 %1.5 %
 
Descriptive Properties
Binder Silicate
Mixing Water Usage 6.8 liters to 25 kg
Package Weight25 kgUnit weight, all included. Plastic sack with dry mix.
Pyrometric Cone Equivalent1585°CASTM C24-89, ORTON cones
Recommended Joint Thickness3.0-5.0 mm
Setting Mechanism air and heat-setting
Typedry mix
Usage 110 kgQuantity to set 1m3 (35.31 ft3) of Bricks
 5.33 kgQuantity to fix 1m2 (11 ft2) of Slabs

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
World Minerals Celite® Super Fine® Super Floss Diatomaceous Earth Antiblock Additive
Superior Flux Superior No. 601B Silver Brazing Paste Flux
Sinotek Materials ZSLG99 High Carbon Graphite
SGL Carbon Group CF 1135 Carbon Filler
PPT BP2000 NiZn Ferrite Powder

CSKAM026 / 2177

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.