MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Applied Silicone 40000 Dimethyl Silicone Elastomer Dispersion in Xylene, Implant Grade
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Solvent Base Elastomer

Information provided by Applied Silicone Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 g/cc1.10 g/cc
Solids Content 35 %35 %
Viscosity 3500 cP3500 cP
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 3535Typical
 31 - 4531 - 45
Tensile Strength >= 8.27 MPa>= 1200 psi
 12.4 MPa1800 psiTypical
Elongation at Break >= 650 %>= 650 %
 800 %800 %Typical
200% Modulus 1.17 MPa
@Strain 200 %
170 psi
@Strain 200 %
Tear Strength >= 17.5 kN/m>= 100 pli
 32.4 kN/m185 pliTypical
 
Processing PropertiesMetricEnglishComments
Cure Time 60.0 min
@Temperature 150 °C
1.00 hour
@Temperature 302 °F
 
Descriptive Properties
Cure SystemPlatinum

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Applied Silicone 40155 Ultra Soft Liquid Silicone Rubber, 000-50 Durometer, Implant Grade

PNUSILA922 / 194591

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.