MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Aluminum Antimonide, AlSb
Categories: Ceramic; Phosphide/Pnictide; Other Engineering Material; Semiconductor

Key Words: Pnictide; Semiconductor; Aluminium Antimonide; Antimony
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 4.218 g/cc
a Lattice Constant 6.1355 Å
Molecular Weight 148.742 g/mol
Volume Compressibility, 10^-10 m²/N 0.571
 
Mechanical PropertiesOriginal ValueComments
Knoop Microhardness 4000N/mm²
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 11
Band Gap 1.6 eV
Electron Mobility, cm²/V-s 200 - 400
Hole Mobility, cm²/V-s 550
 
Thermal PropertiesOriginal ValueComments
CTE, linear 4.20 µm/m-°C
@Temperature 20.0 °C
Thermal Conductivity 60.0 W/m-K
Melting Point 1057 °C
Heat of Formation 585 kJ/mol
Debye Temperature 19.0 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 3.20
 3.20
 
Descriptive Properties
CAS Number25152-52-7
Crystal StructureCubicSphalerite Structure - Space Group F(-4)3m

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mateck GaAs
Mateck Gallium Arsenide (GaAs)
Mateck Zinc Sulphide, ZnS
Silicon, Si
Aluminum Arsenide, AlAs

DSEM00 / 2917

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.