MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Master Bond EP30TC Two component, room temperature curing, thermally conductive epoxy
Categories: Polymer; Thermoset; Epoxy; Epoxy, Thermally Conductive

Material Notes:
  • Highly thermally conductive filler
  • Applicable in very thin bond lines
  • Superior electrical insulation properties
  • NASA low outgassing
Master Bond EP30TC is a multifaceted epoxy for use in thermal management applications. It is a specialty formulation that can be used for bonding, coating, sealing and encapsulation. When used as an adhesive, the thermally conductive filler has very fine particle sizes; subsequently, it can be applied in sections as thin as 5-15 microns. Since it has a lower viscosity and excellent flow properties, it is a good fit for coating and potting. EP30TC has a forgiving ten to one mix ratio by weight. It will cure in 2-3 days at room temperature or in 2-3 hours at 150-200°F. To optimize properties, the recommended cure schedule is overnight at room temperature followed by 2-3 hours at 150-200°F. EP30TC bonds well to a variety of substrates including metals, composites, ceramics, glass and many plastics. As mentioned previously, it has a specialty type filler that allows it to be applied in very thin sections. When this property is combined with its inherent high thermal conductivity, the net result is significantly lower thermal resistance, 7-10 x 10-6 K•m2/W; much less than standard thermally conductive epoxies. Some other desirable features of EP30TC are its outstanding electrical insulation, very low shrinkage upon curing, excellent dimensional stability and low CTE. Prior to mixing, EP30TC should be refrigerated but not frozen. The service temperature range is -100°F to +300°F. The color of Part A is gray and Part B is clear. This sophisticated system can be used in applications in aerospace, electronic, optical and OEM applications.

Product Advantages:

  • Lower viscosity, good flow properties
  • High thermal conductivity and electrical insulation
  • Can be applied in very thin sections
  • Exceptional compressive strength
  • Outstanding abrasion resistance
  • Meets NASA low outgassing specifications

Information provided by Masterbond.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Viscosity 280 - 500 cP280 - 500 cPPart B
 14000 - 28000 cP14000 - 28000 cPPart A
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 85 - 9585 - 95
Tensile Strength 34.5 - 41.4 MPa5000 - 6000 psi
Tensile Modulus 3.45 - 3.79 GPa500 - 550 ksi
Compressive Strength 165 - 179 MPa24000 - 26000 psi
Adhesive Bond Strength 4.14 - 5.52 MPa600 - 800 psilap shear, Al/Al
Taber Abrasion, mg/1000 Cycles 54.154.1CS-17 wheel
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+14 ohm-cm>= 1.00e+14 ohm-cm
Dielectric Constant 4.7
@Frequency 60 Hz
4.7
@Frequency 60 Hz
Dielectric Strength >= 15.7 kV/mm
@Thickness 3.17 mm
>= 400 kV/in
@Thickness 0.125 in
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 149 °C300 °F
Minimum Service Temperature, Air -73.3 °C-100 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  120 - 180 min
@Temperature 93.3 °C
2.00 - 3.00 hour
@Temperature 200 °F
 2880 - 4320 min
@Temperature 23.9 °C
48.0 - 72.0 hour
@Temperature 75.0 °F
Working Life 90.0 - 120 min90.0 - 120 minAfter mixing, 100 g batch
Shelf Life 6.00 Month
@Temperature 4.44 - 10.0 °C
6.00 Month
@Temperature 40.0 - 50.0 °F
In original unopened containers
 
Descriptive Properties
Cure scheduleOvernight at 75°F plus 2-3 hours at 150-200°FOptimum
Mixing Ratio10:1Parts A to B, by weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Master Bond EP42HT-2AO Two Component, Thermally Conductive, Heat Resistant Epoxy
Master Bond EP30AN Thermally Conductive Dimensionally Stable Epoxy System
Master Bond EP21TDC-2AO Flexibilized, Thermally Conductive Two Component Epoxy
Master Bond EP21TDC-2AN Two Component, Flexibilized, Highly Thermally Conductive, Electrically Insulating Epoxy Resin
Master Bond EP21TDC-2 Highly Flexible Cryogenic Epoxy Compound

PMASTM714 / 233771

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.