MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Fujipoly Industries Zebra® Silver Connector
Categories: Polymer; Thermoset; Silicone

Material Notes: Fujipoly New High performance Silver Zebra connectors are constructed of alternating parallel layers of electrically conductive and nonconductive silicone elastomer. The electrically conductive layer if filled with silver metal particles.

Information provided by Fujipoly Industries

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 30Support Rubber
 58Insulating Layer
 80Conductive Layer
Tensile Strength, Yield 2.00 MPaConductive Layer
 4.00 MPaSupport Rubber
 7.70 MPaInsulating Layer
Elongation at Yield 120 %Conductive Layer
 380 %Insulating Layer
 400 %Support Rubber
Tear Strength 13.0 kN/mConductive Layer
 17.0 kN/mInsulating Layer
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 0.00010 ohm-cmConductive Layer
 1.00e+14 ohm-cmSupport Rubber
 1.00e+14 ohm-cmInsulating Layer
Surface Resistance 1.00e+12 ohmBetween Layers
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 85.0 °C
Minimum Service Temperature, Air -40.0 °C
 
Descriptive Properties
ColorLight BlueSupport Rubber
 Off-WhiteInsulating Layer
 Silver GrayConductive Layer
Continuity Resistance<0.5 ohms
Current Carrying Capacity700 mA1.0mm pitch; 0.50mm by 0.50mm pad

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Potters Industries Conduct-O-Fil® S3000-S Silver-Coated Solid Glass Spheres
Aluminum 384.0-F Die Casting Alloy

PFUJIP07 / 39140

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.