MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Chevron Phillips EA6740 Rubber Modified Polystyrene  (discontinued **)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: Description

Chevron EA6740 is a high impact polystyrene material developed for packaging applications. Its processing characteristics make EA6740 excellent for extrusion and deep-draw thermoforming. This material provides good surface smoothness, moderately high heat distortion and excellent practical toughness. The excellent elongation and flexibility properties make EA6740 superior to most common extrusion grades in practical toughness.

Applications

Chevron EA6740 is recommended for such applications as ice cream containers, container lids, cups for hot and cold drinks, conical cup liners, individual portion containers, dairy containers, box liners and medical trays. Information provided by Chevron Phillips Chemical Company.

The Chevron Phillips polystyrene product line was transferred to Americas Styrenics in 2008.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.03 g/ccASTM D792
Melt Flow 3.2 g/10 minCondition G; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 86ASTM D785
Tensile Strength at Break 2600 psiat 2.0 in/min; ASTM D638
Tensile Strength, Yield 2400 psiat 2.0 in/min; ASTM D638
Elongation at Break 85 %ASTM D638
Tensile Modulus 230000 psiASTM D638
Izod Impact, Notched 2.00 ft-lb/in1/4 in. at 73°F; ASTM D256
 2.30 ft-lb/in1/8 in.; ASTM D256
 1.30 ft-lb/in
@Temperature -17.8 °C
0.125 in (3.2 mm) sample; ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 185 °FUnannealed specimen; ASTM D648
Vicat Softening Point 213 °FASTM D1525

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
M. Holland Company MTEGRITY™ GS230 Polystyrene, General Purpose
Ineos Nova 1300 High Heat Crystal Polystyrene
SYNTHOS Krasten® 137 General Purpose Polystyrene
Supreme Petrochem SC 201E General Purpose Polystyrene
Kostat ICP-STAT ICS-1003 PS Sheet

PPSRA08 / 58238

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.