MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

Radici RADILON® ADLINE CS CF10 HP BK Nylon 6/66, 10% Carbon Fiber Reinforced, Conditioned
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66

Material Notes: Description: PA6/66 copolymer 10% carbon fiber reinforced for 3D Printing Fused Deposition Modeling. Suitable for parts requiring stiffness, high dimensional stability and very reduced shrinkage. The material offers good surface aspect and easy processability.

Processing: 3D Printing, Injection Molding

Delivery Form: Granules, Filament

Special Characteristics: Improved Dimensional Stability, High Surface Aspect

Industries: Consumer Industry Goods

Regional Availability: North America, Europe, Asia Pacific, South and Central America, Near East/Africa

Information provided by Radici Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.16 g/cc0.0419 lb/in³ISO 1183
Water Absorption 9.0 %
@Thickness 2.00 mm
9.0 %
@Thickness 0.0787 in
Immersion at 23°C; ISO 62
Moisture Absorption 2.60 %
@Thickness 2.00 mm
2.60 %
@Thickness 0.0787 in
50% RH; ISO 62
 
Thermal PropertiesMetricEnglishComments
Melting Point 195 °C383 °FISO 11357-1/-3
 
Processing PropertiesMetricEnglishComments
Melt Temperature 250 - 280 °C482 - 536 °F
Mold Temperature 70.0 - 100 °C158 - 212 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PRADICI090 / 313591

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.