MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Excelite Plastic Frosted Polycarbonate sheet
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: Frosted PC solid sheet is treated with Special high level of glazing and frosted performance. The visual of the sheet is translucent and can diffuse the light. Of course, the impact resistance of Frosted sheet is excellent.

Features:

  • High Impact Resistance, practically unbreakable
  • Anit-ultraviolet, delay aging
  • UV Resistant
  • 10 year Warranty
  • Lightweight
  • Large range of sheet sizes & thicknesses
Applications
  • Machine Guards
  • Carport and awnings
  • Indoor partition and ceiling
  • Lighting Roofing
  • Safety and security glazing
  • Advertising billboard
  • Indoor decoration and partitic

Information provided by Excelite Plastic Limited

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccGB/T 1033
Water Absorption 0.30 %
@Time 86400 sec
0.30 %
@Time 24.0 hour
GB/T 1033
Thickness 1500 - 12000 microns59.1 - 472 mil
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 60.3 MPa8750 psiGB/T 1040
Elongation at Break >= 90 %>= 90 %GB/T 1040
 108 %108 %Tensile; GB/T 1040
Elongation at Yield 6.0 %6.0 %GB/T 1040
Modulus of Elasticity 0.240 GPa34.8 ksiGB/T 9341
 
Thermal PropertiesMetricEnglishComments
CTE, linear 63.0 µm/m-°C35.0 µin/in-°FGB/T 1034
 
Descriptive Properties
ColorClear, Opal, Red, Yellow, Bronze, Blue, etc.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Excelite Plastic Polycarbonate Light Diffusion sheet

PEXLT005 / 198715

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.