Low-density polyethylene D4041-P is a recommended for use in the boardstock coating industry for applications such as breadboard, cupstock, and liquid packaging board. This resin has low neck-in and good drawdown characteristics. Coatings produced from it exhibit excellent heat-sealing characteristics. List of Applications: - Food-contact applications
- Photographic paper
Information supplied by the manufacturer. Information from manufacturer data sheet. Eastman Chemical Company sold its polyethylene business to Westlake Chemical Corporation in Dec. 2006. This grade no longer appears in the Westlake product line. |
Low neck-in and good drawdown characteristics |