MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Geon® Performance Solutions Vinyl Wire & Cable JC156HN Polyvinyl Chloride, Flexible
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Wire and Cable Grade

Material Notes: Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.

Geon Performance Solutions was created from PolyOne in 2019.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.37 g/cc1.37 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 848415 sec; ASTM D2240
Tensile Strength, Yield 19.3 MPa2800 psiType IV, 510 mm/min; ASTM D638
Elongation at Break 380 %380 %Type IV, 510 mm/min; ASTM D638
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.30e+14 ohm-cm1.30e+14 ohm-cmASTM D257
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -25.0 °C-13.0 °FASTM D746
Oxygen Index 32 %
@Thickness 1.91 mm
32 %
@Thickness 0.0752 in
ASTM D2863
 
Descriptive Properties
AdditiveLead Stabilizer
Change in Flexural Strength97%ASTM D543; 100°C, 1.91 mm; in IRM 902, 4 hr
Change in Ultimate Elongation54%ASTM D543; 100°C, 4 hr, in IRM 902 Oil; 0.075 in
FormsPellets
Generic MaterialPVC, Flexible
Generic NamePolyvinyl Chloride, Flexible
Processing MethodExtrusion Coating
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
Retention of Tensile Elongation85%121°C, 1.91 mm; 336 hr, UL Standard
Retention of Tensile Strength96%121°C, 1.91 mm; 336 hr, UL Standard
UsesWire & Cable Applications
Wire TypesPLTC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Momentive Performance Materials Silopren™ LSR 2003 Liquid Silicone Rubber - General Purpose
International Mold Steel Superplast® Stainless Plastic and Rubber Mold Steel
Garlock 502 Silicone Sheet Rubber
Elkem (Bluestar Silicones) SILBIONE® LSR 4301 Liquid Silicone Rubber
Elkem (Bluestar Silicones) CAF® 731 Silicone Rubber

PH0POL0737 / 145306

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.