MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Wacker Elastosil® R 805/75 Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Vulcanizates made from ELASTOSIL® R 805/75 are noted for their good resistance to motor oils and aggressive mineral oils, even at high temperatures. They have good mechanical properties and a low compression set.

Application: ELASTOSIL® R 805/75 are specially recommended for the production of shaft seals.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.36 g/cc0.0491 lb/in³DIN 53479
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8080curing agent C1; DIN 53505
Tensile Strength at Break 6.40 MPa928 psicuring agent C1; DIN 53504 S1
Elongation at Break 170 %170 %curing agent C1; DIN 53504 S1
Rebound 40 %40 %curing agent C1; DIN 53512
Tear Strength 15.0 kN/m85.6 plicuring agent C1; ASTM D624 B
Compression Set 17 %
@Temperature 175 °C,
Time 79200 sec
17 %
@Temperature 347 °F,
Time 22.0 hour
curing agent C1; DIN ISO 815-B
 
Processing PropertiesMetricEnglishComments
Cure Time 15.0 min
@Treatment Temp. 165 °C
0.250 hour
@Treatment Temp. 329 °F
 
Descriptive Properties
Appearancebeige

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Silicone Rubber
Overview of materials for Liquid Silicone Rubber

PWACK9245 / 204774

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.