Pro-fax PH835 polypropylene homopolymer is available in pellet form. This resin is typically used in spun bond and continuous filament applications that require superior spinnability and finer fibers. PH835 is also used in extrusion coating applications. Applications: Food Packaging Film, Hygiene Nonwoven, Intermediate Bulk Containers, Protective Clothes, Wipes/Tissues.Information provided by LyondellBasell. |