MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Phillips 66 Marok® ISO Grade 100
Categories: Fluid; Lubricant

Material Notes: Marok is a high-quality, adhesive, extreme-pressure (EP) lubricant specifically developed to lubricate in the presence of moisture or where oil leakage is a problem. It is recommended for the lubrication of marine, mining and industrial equipment operating in wet environments, and for the lubrication of air-powered tools such as rock drills and jackhammers. Marok is formulated with naphthenic base oils and a specially tailored additive package to provide excellent protection for pneumatic percussion tools and marine and industrial equipment operating under wet conditions. It has good load-carrying capacity to protect against wear and seizure of sliding metal surfaces under heavy or shock-load conditions. It has excellent adhesion to metal surfaces in the presence of moisture, and protects against rust and corrosion. It resists dripping and leakage, which is especially useful in applications where bearing clearances are large or seals are inadequate.

Applications:

  • Pneumatic percussion tools such as jackhammers, pavement breakers and rock drills
  • Mining equipment such as demolition hammers, chipping hammers and drifters
  • Marine applications such as stern tube bearings, oil-lubricated tunnel bearings, and cylinder lubricant for steam engines and crosshead engines
  • Drive chains and overhead conveyors where a non-drip lubricant is required
  • Enclosed industrial gear drives where oil leakage is a problem
Features/Benefit:
  • Good extreme-pressure properties
  • Protects against wear and seizure
  • Excellent adhesion to metal surfaces in the presence of moisture
  • Resists dripping and leakage
  • Protects against rust and corrosion
  • Low odor

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.922 g/cc0.922 g/cc
Density 0.920 g/cc0.0332 lb/in³
Viscosity Measurement 5151Index
Saybolt Viscosity at 100°F 530 SUS530 SUS
Saybolt Viscosity at 210°F 57.4 SUS57.4 SUS
Kinematic Viscosity at 40°C (104°F) 100 cSt100 cSt
Kinematic Viscosity at 100°C (212°F) 9.2 cSt9.2 cSt
ASTM Color 3.53.5ASTM D1500
 
Chemical PropertiesMetricEnglishComments
Total Acid Number 0.600.60[mg KOH/g]; ASTM D974
 
Mechanical PropertiesMetricEnglishComments
Four Ball Extreme Pressure, Weld Load 250 kg551 lb (mass)ASTM D2783
Four Ball Wear 0.320 mm0.0126 inScar Diameter; ASTM D4172
Falex Load Test 408000 g900 lbEP; ASTM D3233
 
Thermal PropertiesMetricEnglishComments
Pour Point -21.0 °C-5.80 °F
Flash Point 192 °C378 °FCOC
 
Descriptive Properties
Carbon Residue0.1%ASTM D524

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WCON5186 / 198439

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.