MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Chevron Phillips 4522 LDPE Shrink and Heavy Duty Packaging Film Resin  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: Resin Type: Homopolymer

Characteristics: Excellent Tensile Strength, Excellent Impact Strength, Very Good Tear Resistance, Very Good Abrasion Resistance, No Slip, No Antiblock

Applications:Pallet Shrink Wrap, Heavy Duty Packaging

Processing Conditions: Extruder 6.35 cm. Screw L/D Ratio 24:1. Die Opening 0.0762 cm. Blow-Up Ratio 3:1.

Film properties below based on film thickness of 76 µm.

Data provided by Chevron Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.923 g/cc0.0333 lb/in³ASTM D1505
Melt Flow 0.50 g/10 min0.50 g/10 minCondition E; ASTM D 1238
 
Mechanical PropertiesMetricEnglishComments
Secant Modulus, MD 0.170 GPa24.7 ksiASTM D882
Secant Modulus, TD 0.180 GPa26.1 ksiASTM D882
Coefficient of Friction >= 1.0>= 1.0ASTM D1894
Dart Drop 2.80 g/micron71.1 g/milF50; 2 in. dart/60 in. drop height; ASTM D 1709
 
Optical PropertiesMetricEnglishComments
Haze 9.5 %9.5 %ASTM D2457
Gloss 59 %59 %at 45°. ASTM D 2457
 95 %95 %at 60°. ASTM D 2457
 
Processing PropertiesMetricEnglishComments
Melt Temperature 210 °C410 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ravago Manufacturing Americas Hylon® N1033HL Nylon 6/6 (Cond)
PlastiComp Complet® LGF60 - PA66 Nylon 66, 60% Long Glass Fiber Reinforced
EMS-Grivory Grivory® GTR 45 PA6I/6T
DuPont Mobility and Materials Zytel® ST801 BK010A PA66-HI
Clariant Renol 612-01L Nylon 612, Lubricated

PCHEVV80 / 20476

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.