MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Magnesium
Magnesium Elektron - Service & Innovation in Magnesium

Magnesium Elektron Elektron® AZ91D Magnesium Alloy
Categories: Metal; Nonferrous Metal; Magnesium Alloy

Material Notes:

Information provided by Magnesium Elektron.

Vendors: Magnesium Elektron is the world leader in high strength magnesium alloys in rolled, extruded and cast forms. Phone (303) 589-3189 or visit www.magnesium-elektron.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 120 MPa17400 psi
Tensile Strength, Yield 120 MPa
@Strain 0.2 %
17400 psi
@Strain 0.2 %
Elongation at Break 3.0 %3.0 %
Compressive Yield Strength 160 MPa
@Strain 0.2 %
23200 psi
@Strain 0.2 %
Fatigue Strength 100 MPa
@# of Cycles 5.00e+7
14500 psi
@# of Cycles 5.00e+7
Unnotched Rotating Bend
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 9.0 %9.0 %
Magnesium, Mg 90.2 %90.2 %As Balance
Manganese, Mn 0.30 %0.30 %
Zinc, Zn 0.50 %0.50 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Magnesium AZ91D-F, Cast
Parkway Products Thixomolded® AZ91D Magnesium
Aluminum A360.0-F Die Casting Alloy
Magnesium Elektron Elektron® AZ91 Magnesium Alloy
SAE AZ91 Magnesium Matrix Composite, as cast

NMAGEL941 / 186956

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.