MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

LyondellBasell Moplen HP520J Polypropylene  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: LyondellBasell Australia’s Polypropylene grade HP520J is a medium flow homopolymer with a conventional molecular weight distribution and is formulated with a general-purpose additive package. HP520J is designed for the production of biaxial oriented films (BOPP) for high quality packaging and laminates. HP520J gives reliable and consistent processing on BOPP stenter lines, providing films having high transparency and gloss, with a good balance of film properties. Applications: Food Packaging Film

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³Method D; ISO 1183-1
Melt Flow 3.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
3.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7575ISO 868
Tensile Strength, Yield 33.0 MPa4790 psiISO 527-1,-2
Flexural Modulus 1.50 GPa218 ksiISO 178
Izod Impact, Notched (ISO) 5.00 kJ/m²
@Temperature 23.0 °C
2.38 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1A
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C194 °Funannealed; ISO 75B-1,-2
Vicat Softening Point 155 °C311 °FISO 306
 
Descriptive Properties
Processing MethodBOPP

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ineos H12E-00 Polypropylene Homopolymer, Antistatic
Ineos H07D-00 Polypropylene Homopolymer
Braskem TI60035NB High Impact Copolymer Polypropylene
Braskem FP450WV Polypropylene Homopolymer
Braskem FF650WV Homopolymer Polypropylene

PEQT9030 / 220661

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.