MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

NuSil MED-4750 Two-Part Standard High Consistency Elastomers - Unrestricted Medical Use
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Description: High consistency rubber, or HCR, consists of high molecular weight polymer combined with silica to produce a material that can be molded, extruded, or calendared into a useful end product. An HCR has the consistency of clay and is primarily formulated in a one or two part system (peroxide and platinum catalysts, respectively).

Important Properties of Adhesives: Most platinum cure high consistency rubbers are two component systems with an easy-to-work-with 1:1 mix ratio. Features of platinum cure high consistency rubbers include the following:

  • Two part (typically)
  • Heat accelerated
  • No byproducts
  • Post cure optional
  • Low percent shrinkage
Comments: High Tear

Cure System: Platinum

Information provided by NuSil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.16 g/cc1.16 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5050Typical
 45 - 5545 - 55Certified
Tensile Strength at Break 8.30 MPa1200 psiCertified
 10.0 MPa1450 psiTypical
Tensile Stress at Strain 2.07 MPa
@Strain 200 %
300 psi
@Strain 200 %
Elongation at Break 750 %750 %Certified
 1000 %1000 %Typical
Tear Strength 35.1 kN/m200 pliCertified
 43.8 kN/m250 pliTypical
 
Processing PropertiesMetricEnglishComments
Cure Time 10.0 min
@Temperature 116 °C
0.167 hour
@Temperature 241 °F
Working Life 120 min
@Temperature 25.0 °C
120 min
@Temperature 77.0 °F
 
Descriptive Properties
Plasticity100 mils

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
NuSil MED-4770 Ultra High Performance High Consistency Elastomers - Unrestricted Medical Use
Dow Silastic® MEDICAL ADHESIVE SILICONE, TYPE A
NuSil MED-6350 Gel - Restricted Medical Use
Overview of materials for Silicone Rubber
Dow Silastic® Q7-4750 BIOMEDICAL GRADE ETR ELASTOMER, KIT

PNUSIL312 / 142036

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.