MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Eastman EastaPure™ PM Acetate Solvent
Categories: Fluid; Solvent

Material Notes: CAS No. 108-65-6

Product Description: Eastman EastaPure™ PM acetate (propylene glycol monomethyl ether acetate) is a slow evaporating solvent with both ether and ester functional groups. It is a colorless liquid with a mild odor. Eastman EastaPure™ PM acetate solvent is being offered for photoresist formulations. PM acetate can also be used in edge bead removal after spin coating processes.

Application/Uses:

  • Advanced resist
  • Developers
  • Edge bead removal
  • Flat Panel/LCD
  • LED/OLED
  • Microelectronics
  • Negative tone resist
  • Photolithography
  • Photoresist
  • Photoresist stripper applications
  • Positive tone resist
  • Semiconductors
  • Solvents
Key Attributes:
  • Excellent resin solubility
  • High assay
  • High Purity/Low Trace Metals
  • Viscosity control

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.968 - 0.971 g/cc0.0350 - 0.0351 lb/in³
Viscosity 1.07 cP1.07 cPNeat
 1.1 cP1.1 cPLiquid
Molecular Weight 132.2 g/mol132.2 g/mol
Vapor Pressure  0.00373 bar
@Temperature 20.0 °C
2.80 torr
@Temperature 68.0 °F
 0.0300 bar
@Temperature 55.0 °C
22.5 torr
@Temperature 131 °F
Surface Tension 26.4 dynes/cm26.4 dynes/cm
 
Chemical PropertiesMetricEnglishComments
Critical Pressure 30.1 bar22600 torr
Critical Temperature 324.7 °C616.5 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 540 µm/m-°C300 µin/in-°F
Melting Point -67.0 °C-88.6 °FFreezing Point
Boiling Point 140 - 150 °C284 - 302 °F@ 760 mm Hg
Flash Point 46.0 °C115 °FSetaflash Closed Cup
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.401.40
 
Descriptive Properties
ColorPT-Co
Upper Limits for Trace Metals10 ppbAluminum
 10 ppbBarium
 10 ppbCadmium
 10 ppbCalcium
 10 ppbChromium
 10 ppbCobalt
 10 ppbCopper
 10 ppbGallium
 10 ppbGermanium
 10 ppbIron
 10 ppbLead
 10 ppbLithium
 10 ppbMagnesium
 10 ppbManganese
 10 ppbNickel
 10 ppbPotassium
 10 ppbSilver
 10 ppbSodium
 10 ppbStrontium
 10 ppbTitanium
 10 ppbZinc

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Eastman EastaPure™ EP Solvent

PEATM5148 / 222342

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.