MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Wacker Vinnapas® 4042 H Vinyl Acetate-Ethylene Copolymer
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate

Material Notes: Product description: VINNAPAS® 4042 H is a very flexible dispersible polymer powder based on vinyl acetate and ethylene with slight hydrophobic effect for very good tensile adhesion strength particularly on organic surfaces.

Properties: VINNAPAS® 4042 H is a copolymer powder based on vinyl acetate and ethylene and is dispersible in water. VINNAPAS® 4042 H is a polymeric binder and also provides a slight hydrophobic effect. Blended with inorganic binders the powder will provide very good workability; cured mortars with VINNAPAS® 4042 H have improved adhesion, flexibility, deformability and abrasion resistance. Due to the high ethylene content and therefore low glass transition temperature (Tg), this copolymer is highly flexible. Mortars modified with VINNAPAS® 4042 H will have a lasting effect on water absorption and water repellency. VINNAPAS® 4042 H will not have any effect on water-vapor transmission at common dosages. VINNAPAS® 4042 H contains a fine mineral filler as an antiblocking agent.

Special features: VINNAPAS® 4042 H is a dispersible polymer powder in the lower Tg range with a slight hydrophobic effect. It has no effect on rheology. Mortars modified with VINNAPAS® 4042 H exhibit very good workability and attain high strength when cured. Additionally VINNAPAS® 4042 H provides slight hydrophobicity within the hardened mortar. It is especially suitable for adhesive mortars and embedding mortars in ETICS.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.400 - 0.550 g/ccDIN EN ISO 60
Solids Content >= 98 %
Particle Size 400 µmmax 4% over; DIN EN ISO 4610
Ash <= 15 %
@Treatment Temp. 1000 °C
 
Descriptive Properties
Appearancewhite to light beige powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PWACK9602 / 205131

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.