Greenflex MP 35 is an ethylene vinyl acetate copolymer (EVA) for injection molding and extrusion. Greenflex MP 35 is an easy flowing material and provides a very high elasticity. Main Applications: Greenflex MP 35 is recommended for the production of articles requiring a high degree of elasticity, such as flippers. Information provided by Polimeri Europa. Versalis is the Eni subsidiary containing the plastics and rubber businesses. |