MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Sipol Technipol® PA 162 Thermoplastic Adhesive Co-polyamide
Categories: Polymer; Adhesive; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Description: Technipol® PA 162 is a thermoplastic adhesive co-polyamide based extruded into rod shape and used by automatic lasting machines in the footwear industry. This polyamide rod cement has been specifically designed to be also used on the new toe lasting machines, equipped with tracers. Thanks to its quick setting time, its good flexibility, its excellent wettability and its high adhesion to leather and to both synthetic and regenerated materials, Technipol® PA 162 is the ideal adhesive for the shoe manufacturing. Due to the wide variety of materials used in the today’s footwear construction, it is recommended to run some preliminary trials in order to homologate the Technipol® PA 162. Finally, Technipol® PA 162 contains more than 80% of raw materials coming from renewable resources (no food grade).

Information provided by SIPOL SpA

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Brookfield Viscosity 8.0 cP
@Temperature 232 °C
Cone/ plate Viscometer, Model Brookfield CAP 2000+.; MI 12
Storage Temperature 5.00 - 10.0 °C
 
Thermal PropertiesOriginal ValueComments
Softening Point 190 °CASTM D 3461
 
Processing PropertiesOriginal ValueComments
Shelf Life 18.0 Month
 
Descriptive Properties
ColorAmber
Diameter3.8-4.0 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSIPOL009 / 297134

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.