MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Wacker R2000/60 Silicone Rubber Base
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: R2000/60 Silicone Rubber Base is a 60 durometer, general purpose base.

Special features:

  • Good tensile strength
  • Good elongation
  • Good tear resistance
  • Good calendering qualities
  • Excellent molding qualities
  • Excellent shelf stability

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5757ASTM D2240
Tensile Strength at Break 9.20 MPa1330 psiASTM D412
Elongation at Break 558 %558 %ASTM D412
Tear Strength 24.7 kN/m141 pliASTM D624 die B
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -73.0 °C-99.4 °FASTM D746
 
Processing PropertiesMetricEnglishComments
Cure Time 10.0 min
@Treatment Temp. 171 °C
0.167 hour
@Treatment Temp. 340 °F
press cured
 
Descriptive Properties
AppearanceOff-white

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PWACK9250 / 204779

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.