MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Lubrizol Estane® D91T80 NAT 01 Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Type: Aliphatic polycaprolactone based Thermoplastic Polyurethane (TPU) with a 81 Shore A Hardness.

Features: Translucent resin with excellent colour stability upon UV exposure

Uses: Injection molding outdoor applications.

Information provided by The 159 Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.11 g/cc1.11 g/ccISO 2781 / ASTM D-792
Maximum Moisture Content 0.0200.020
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 81
@Time 3.00 sec
81
@Time 0.000833 hour
ISO 868
Tensile Strength 25.3 MPa3670 psiISO 527-2 / ASTM D-412
Elongation at Break 800 %800 %ISO 527-2 / ASTM D-412
100% Modulus 4.30 MPa
@Strain 100 %
624 psi
@Strain 100 %
ISO 527-2 / ASTM D-412
300% Modulus 7.50 MPa
@Strain 300 %
1090 psi
@Strain 300 %
ISO 527-2 / ASTM D-412
Tear Strength 80.0 kN/m456 pliISO 34-1B (ASTM D-624 Die C)
Abrasion 3030[mm3]; ISO 4649
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 60.0 °C140 °FA50; ISO 306
 
Optical PropertiesMetricEnglishComments
Haze 23 %
@Thickness 2.00 mm
23 %
@Thickness 0.0787 in
ASTM 1003
 
Processing PropertiesMetricEnglishComments
Feed Temperature 175 °C347 °F
Nozzle Temperature 190 °C374 °F
Zone 2 180 °C356 °F
Zone 3 185 °C365 °F
Mold Temperature 35.0 °C95.0 °F
Drying Temperature 80.0 - 90.0 °C
@Time 7200 sec
176 - 194 °F
@Time 2.00 hour
Moisture Content <= 0.10 %<= 0.10 %MQSA 44
Dew Point -40.0 °C-40.0 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLUBR5020 / 238890

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.