Description: PLEXIGLAS® XT extruded acrylic has the following properties:- absolutely colorless and clear
- break-resistant to impact-resistant (PLEXIGLAS RESIST®)
- unequalled resistance to weathering and ageing
- very good surface; brilliant, textured or satin (PLEXIGLAS SATINICE®)
- sheets, tubes, round rods, multi-skin sheets, corrugated sheets, mirror sheets
- 1.5 to 25 mm solid sheet thickness, multi-skin sheets 16 mm and 32 mm thick
- standard size up to 4050 x 2050 mm (+ extra lengths)
- more than 25 standard colors
- good resistance to dilute acids
- limited resistance to organic solvents
- good resistance to alkalis
- easy to work, similar to hardwood
- easy to thermoform under optimal constant conditions
- easily bonded also with solvent adhesives (e.g. ACRIFIX® 116, 117)
- burns more or less like hardwood; very little smoke generation
- max. service temperature approx. 70 °C
Specific Notes for this Material: Standard grades for solid sheets with higher, graded impact strength and reduced rigidity, UV absorbing. Information provided by degussa. The former Evonik Methacrylates business has been sold to Röhm GmbH (Roehm). |