MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Tra-Con Tra-Bond 2162D Color Coded Smooth Paste Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: TRA-BOND 2162D epoxy system is color-coded for easy mixing and handling as a smooth paste, and it develops strong bonds to most materials including metals, glass, ceramics, leather, wood, concrete and many plastics exhibits medium shrinkage during cure and has good dimensional stability over a wide temperature range. Fully cured TRA-BOND 2162D is a tough, durable, high peel, semi-flexible electrically insulating adhesive with good low temperature mechanical, thermal shock and impact resistance properties. In addition, it provides good resistance to gases and vapors, weather, water, salt solutions, petroleum solvents and lubricants, gasoline, mild acids and alkalis, and other organic and inorganic compounds.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.23 g/cc1.23 g/ccMixed
Viscosity 54000 cP
@Temperature 25.0 °C
54000 cP
@Temperature 77.0 °F
After mixing
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6060
Tensile Strength, Yield 6.89 MPa1000 psi
Elongation at Yield 45 %45 %
Izod Impact, Notched 2.19 J/cm4.10 ft-lb/in
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 4.6
@Frequency 1000 Hz
4.6
@Frequency 1000 Hz
Dielectric Strength 14.2 kV/mm360 kV/in
Dissipation Factor 0.10
@Frequency 1000 Hz
0.10
@Frequency 1000 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 110 µm/m-°C
@Temperature 20.0 °C
61.1 µin/in-°F
@Temperature 68.0 °F
Maximum Service Temperature, Air 110 °C230 °F
Minimum Service Temperature, Air -70.0 °C-94.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 540 min9.00 hour6 hrs @ 25°C + 3 hrs @ 65°C
 1440 min
@Temperature 25.0 °C
24.0 hour
@Temperature 77.0 °F
Pot Life 180 min180 min
 
Descriptive Properties
Color Light Yellow
Mix Ratio, parts by weight100/100Resin/Hardener

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTRAC041 / 70969

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.