MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

ExxonMobil 22M Mobilgear SHC
Categories: Fluid; Lubricant

Material Notes: Mobilgear SHC 22M and 46M are supreme performance ultra high viscosity synthetic lubricants designed specifically for use in heavily loaded, low speed gears where boundary lubrication conditions often prevail. They are formulated from wax-free synthetic base stocks, pioneered by our company, which have remarkable low-temperature fluidity, even at such high viscosity grades. These ultra high viscosity products can be pumped over relatively long distances and use standard spray application equipment. The combination of a naturally high viscosity index and a unique additive system gives the products exceptional thermal/oxidative properties and provides outstanding performance under severe high and low temperature operating conditions even with very slow moving gears. The additive formulation also provides excellent EP and anti-wear performance and rust and corrosion inhibition. Mobilgear SHC 22M and 46M exceed Falk Corporations minimum viscosity requirements for intermittent lubrication of gears - winter and summer grades, respectively. These grades also meet the viscosity requirements for AGMA lubricant numbers 14R and 15R, respectively, although they are not residual lubricants. Mobilgear SHC 22M and 46M do not contain any solvent or any asphaltic-type base oil.

Application Considerations: Normally, conversion to Mobilgear SHC 22M or 46M from asphaltic or grease products will be a simple process with no change in lubricant spray equipment. It is recommended that the gears be thoroughly cleaned to take advantage of the light colour of these synthetic products. Consult your Mobil representative for further details on lubricant conversion. Mobilgear SHC 22M and 46M are designed specifically for use in heavily loaded, low speed open gearing which drive stationary rotating machinery. Product application is by spray nozzle systems. Specific applications include: Kilns and mills in metal mining, cement and limestone production and in sugar plants; Slow speed, heavily loaded plain and rolling contact bearings

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.890 g/cc
@Temperature 15.6 °C
0.890 g/cc
@Temperature 60.1 °F
ASTM D4052
Viscosity Measurement 180180Index; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 22000 cSt22000 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 700 cSt700 cStASTM D445
 
Thermal PropertiesMetricEnglishComments
Pour Point 6.00 °C42.8 °FASTM D97
Flash Point 240 °C464 °FASTM D92
 
Descriptive Properties
Copper Strip Corrosion1B3 hrs @ 100°C
Rust Prevention, Synthetic Sea WaterpassASTM D665B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WEXXON246 / 75671

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.