MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Methylcyclohexane, C7H14
Categories: Fluid; Solvent

Key Words: C7H14
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.774 g/cc
@Temperature 20.0 °C
0.0280 lb/in³
@Temperature 68.0 °F
Viscosity 0.719 cP
@Temperature 20.0 °C
0.719 cP
@Temperature 68.0 °F
Dynamic Viscosity
Molecular Weight 98.189 g/mol98.189 g/mol
Vapor Pressure 0.048277 bar
@Temperature 20.0 °C
36.211 torr
@Temperature 68.0 °F
 
Chemical PropertiesMetricEnglishComments
Critical Pressure 34.8 bar26100 torr
Critical Temperature 299 °C570 °F
Critical Density 0.267 g/cc0.00965 lb/in³
Critical Molar Volume 368 cm³/mol22.5 in³/mol
 
Thermal PropertiesMetricEnglishComments
Heat of Vaporization 317 J/g136 BTU/lb
Specific Heat Capacity 1.373 J/g-°C
@Temperature 25.0 °C
0.3282 BTU/lb-°F
@Temperature 77.0 °F
Vapor
Thermal Conductivity 0.1109 W/m-K
@Temperature 20.0 °C
0.7696 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point -126.6 °C-195.9 °F
Boiling Point 101 °C214 °F
 
Descriptive Properties
Antoine's Vapor Pressure A Parameter15.7105
Antoine's Vapor Pressure B Parameter2926.04
Antoine's Vapor Pressure C Parameter-51.75
Antoine's Vapor Pressure Formulaln πp = A - B/(T+C)P in mmHg and T in K
CAS registry number (CARN)108-87-2
Chemical FormulaC7H14
Critical Compressibility (Zc)0.269
Dynamic Viscosity Formulalog10 η=A(1/T-1/B)
Dynamic Viscosity Parameter A528.41
Dynamic Viscosity Parameter B271.58
Molar Heat Capacity (298K)134.828 J/mol-K
Molar Heat Capacity of Vapor a Parameter-61.8722
Molar Heat Capacity of Vapor b Parameter0.7837
Molar Heat Capacity of Vapor c Parameter-0.0004435
Molar Heat Capacity of Vapor d Parameter9.36E-08
Molar Heat Capacity of Vapor FormulaCp = a + bT + cT2 + dT3Cp in J/mol-K

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil Isopar™ E Isoparaffin Fluid

VORGS251 / 99614

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.