MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Chevron Phillips MarFlex® 7105DL Polyethylene; LLDPE  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: Hexene linear low density polyethylene. This LLDPE is tailored for blown film applications that require:
  • High strength
  • Good drawdown
  • Good processability
  • Use alone or in blends with LDPE or HDPE
  • High amounts of antiblocking agent

Applications: Typical blown film applications include:

  • Industrial liners
  • Heavy duty bags
  • Institutional packaging

Information provided by Phillips

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.918 g/cc0.0332 lb/in³ASTM D-1505
Melt Index of Compound 0.50 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.50 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D-1238
Slip Level 0.00 ppm0.00 ppm
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 500 %500 %Blown Film at 1 mil; ASTM D-882
Film Elongation at Break, TD 660 %660 %Blown Film at 1 mil; ASTM D-882
Coefficient of Friction 1.01.0Blown Film at 1 mil; ASTM D-1894
Elmendorf Tear Strength, MD 15.7 g/micron400 g/milBlown Film at 1 mil; ASTM D-1922
Elmendorf Tear Strength, TD 23.6 g/micron600 g/milBlown Film at 1 mil; ASTM D-1922
Dart Drop 17.7 g/micron450 g/milBlown Film at 1 mil; ASTM D-1709
Film Tensile Strength at Break, MD 45.0 MPa6530 psiBlown Film at 1 mil; ASTM D-882
Film Tensile Strength at Break, TD 36.0 MPa5220 psiBlown Film at 1 mil; ASTM D-882
1% Secant Modulus, MD 200 MPa29000 psiBlown Film at 1 mil; ASTM D-882
1% Secant Modulus, TD 214 MPa31000 psiBlown Film at 1 mil; ASTM D-882
 
Optical PropertiesMetricEnglishComments
Haze 14 %
@Thickness 0.0254 mm
14 %
@Thickness 0.00100 in
blown films; ASTM D-1003
Gloss 80 %80 %60°, Blown Film at 1 mil; ASTM D-2457
 
Descriptive Properties
Process Aid Yes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHEVD227 / 20721

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.