MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Wellman Wellamid® GF1398-BK1 Nylon 66, 30% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes:

All information provided by Wellman Engineered Resins.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.37 g/cc0.0495 lb/in³ISO 1183-87
Linear Mold Shrinkage, Flow 0.0030 - 0.0070 cm/cm0.0030 - 0.0070 in/inDIS 294-4
Linear Mold Shrinkage, Transverse 0.011 - 0.015 cm/cm0.011 - 0.015 in/inDIS 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 165 MPa23900 psiISO 527-93
Elongation at Break 2.0 %2.0 %ISO 527-93
Flexural Strength 225 MPa32600 psiISO 178-93
Flexural Modulus 8.60 GPa1250 ksiISO 178-93
Izod Impact, Notched (ISO) 7.00 kJ/m²3.33 ft-lb/in²ISO 180-93
 
Thermal PropertiesMetricEnglishComments
Melting Point 260 °C500 °FISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 245 °C473 °FISO 75-93

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Techmer ES HiFill® PA6 GF30 L 30% Milled Glass
DuPont Mobility and Materials Zytel® 70G33HSL BK083 PA66-GF33
DuPont Mobility and Materials Zytel® 70G30HSL BK039B PA66-GF30
Domo Technyl® A 218 V30 Nylon 66, 30% Glass Fiber, EH50
Domo Technyl® A 218 V30 Nylon 66, 30% Glass Fiber, EH0

PWEL00144 / 88064

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.