MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Eneos AT400 TPE
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: AT is a syndiotactic 1, 2-polybutadiene and thermoplastics elastomer containing at least 90% 1, 2-bonds, which have a melting point derived from its syndiotactic structure. Blending compounds with AT yields improved processability (compound viscosity, green strength, and mill shrinkage), and physical properties (strength and hardness) of the bead and tread.

Application: Tread, bead

ENEOS has acquired the elastomer product lines from JSR Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.914 g/cc
Mooney Viscosity 24.2
@Temperature 130 °C
ML1+4
Melt Flow 9.0 g/10 min
@Pressure 0.2982 MPa,
Temperature 150 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 94
Tensile Strength 21.2 MPa
Elongation at Break 330 %
100% Modulus 9.90 MPa
300% Modulus 17.1 MPa
 
Thermal PropertiesOriginal ValueComments
Melting Point 126 °C
 
Descriptive Properties
Content (%)94Microstructure Percentage of 1,2 bonds
Product formPellet

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PJSRC8133 / 295449

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.