BMC SLC 2000 is a medium strength, low-cost, glass reinforced polyester compound with adjustable shrinkage. Ideal for circuit breakers, motor switch housings, fuse holders, brush holders, standoff insulators and conduit boxes. UL® recognized. This material was formerly known as Glastic® SLC 2000. |