MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Hyflon® PFA P7010 Perfluoroalkoxy (PFA)
Categories: Polymer; Thermoplastic; Fluoropolymer; Perfluoroalkoxy (PFA); Polyperfluoroalkoxyethylene, Molded/Extruded

Material Notes: Hyflon® PFA P7010 is a clear, semi-crystalline melt processable perfluorinated resin. It is designed for electrostatic powder coatings and is particularly recommended for use as a topcoat in antistick applications.

Hyflon® PFA P7010 exhibits very low surface energy, very low coefficient of friction and excellent thermal and flame resistance Additionally Hyflon® PFA P7010 coatings show excellent smooth surface finish, outstanding antistick behavior and can maintain performance over a wide temperature range.

Main features of Hyflon® PFA P7010 include:
- Very low surface energy
- Excellent antistick behavior
- Very low coefficient of friction
- Very good surface finish
- Outstanding thermal resistance

Applications: Coating Applications

Features: Good Surface Finish; Good Thermal Stability; Low Friction; Semi Crystalline

Processing
- Hyflon® PFA P7010 is intended as a topcoat material to apply to primered substrates. It can be processed using normal electrostatic powder coating techniques. Generally the procedure involves substrate preparation, coating, baking and cooling.
- Hyflon® PFA P7010 can be used neat and without any further formulation. Several passes may be required to obtain the desired PFA load and build up coating thickness without defects.
- Substrate preparation, gun parameters such as voltage and both oven temperature and time must all be well controlled to achieve defect free coated items.

Storage and Handling
- Hyflon® melt processable fluoropolymer resins can be stored without shelf life issues when kept in a clean and dry area at ambient temperatures. Opened containers should be tightly resealed to prevent any contamination.

Safety and Toxicology
- Before using Hyflon® melt processable fluoropolymer resins consult the product Material Safety Data Sheet and follow all label directions and handling precautions.
- As with all fluoropolymer materials, handling and processing should only be carried out in well ventilated areas. Vapor extractor units should be installed above processing equipment. Fumes must not be inhaled and eye and skin contact ought to be avoided. In case of skin contact wash with soap and water. In case of eye contact flush with water immediately and seek medical help. Do not smoke in areas contaminated with powder, vapor or fumes.
- See Material Safety Data Sheet for detailed advice on waste disposal methods.

Packaging
- Hyflon® PFA P7010 is packaged in 10kg non returnable drums. Each drum has two bags liner made of polyethylene resin.

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.16 g/ccASTM D792
Particle Size 25 µmAverage
Melt Flow 10 - 17 g/10 min
@Load 5.00 kg,
Temperature 372 °C
ASTM D1238
 
Thermal PropertiesOriginal ValueComments
Melting Point 300 - 310 °C
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorClear/Transparent
FormsPowder
ProcessingCoating

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y4254 / 280054

http://www.madehow.com/Volume-1/Tire.html

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.