MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Wacker Powersil® XLR® 630 A/B Liquid Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Product description: POWERSIL® XLR® 630 A/B is an especially low viscous, two-component silicone compound with excellent processing properties. The vulcanized rubber is noted for the good mechanical properties as well as for the excellent dielectrical behaviour.

Special features:

  • ready-to-use, two-component system
  • extreme low viscosity as a liquid rubber
  • excellent processing with suitable mixing and dosing equipment
  • very good dielectrical properties
  • high tracking resistance
Application: POWERSIL® XLR® 630 A/B is the right choice for economical production of large articles like hollow core insulators with suitable mixing and dosing equipment. Because of its extreme low viscosity the use of a highcost injection moulding equipment is not necessary, but of course possible if wanted. Due to the outstanding electrical properties POWERSIL® XLR® 630 A/B is an insulating material for indoor as well as for outdoor use.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³ISO 1183-1 A
Viscosity  12000 cP
@Shear Rate 10.0 1/s
12000 cP
@Shear Rate 10.0 1/s
Component B; ISO 3219
 13000 cP
@Shear Rate 10.0 1/s
13000 cP
@Shear Rate 10.0 1/s
Mix; ISO 3219
 14000 cP
@Shear Rate 10.0 1/s
14000 cP
@Shear Rate 10.0 1/s
Component A; ISO 3219
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 3535ISO 868
Tensile Strength at Break 7.00 MPa1020 psiISO 37
Elongation at Break 450 %450 %ISO 37
Tear Strength 25.0 kN/m143 pliASTM D624 B
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Dielectric Constant 2.9
@Frequency 50 Hz
2.9
@Frequency 50 Hz
IEC 60250
Dielectric Strength 23.0 kV/mm584 kV/inIEC 60243
Dissipation Factor 0.00020
@Frequency 50 Hz
0.00020
@Frequency 50 Hz
IEC 60250
Arc Resistance >= 300 sec>= 300 secIEC 61621
 
Processing PropertiesMetricEnglishComments
Cure Time 5.00 min
@Treatment Temp. 165 °C
0.0833 hour
@Treatment Temp. 329 °F
Pot Life 1440 min1440 min
 
Descriptive Properties
Colorlight gray
Track Resistance1A 4.5IEC 60587

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Wacker Powersil® XLR® 630 REEF.CON. A/B Liquid Rubber
Overview of materials for Polyimide, Thermoset Film
Momentive Performance Materials RTV630 Blue General Purpose Potting/Encapsulating Compound
Covestro Texin® 5590 Thermoplastic Polyurethane, Polyether-based, Medical
Celanese Riteflex® 640A TPC, Unfilled

PWACK9398 / 204927

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.