MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Wacker Silfar® 100 Dimethicone/Silicone Fluid
Categories: Fluid

Material Notes: Structural Formula: (H3C)3SI-(OSi(CH3)2-)NOSi(CH3)3

SILFAR® 100 is a polydimethylsiloxane obtained by hydrolysis and polycondensation of dichlorodimethylsilane and chlorotrimethylsilane. The degree of polymerization (n) is such that the mean kinematic viscosity is 100mm²/s at 25°C.

Properties: SILFAR® 100 complies with the requirements set down in the monographs "Dimethicone" (EP) and "Dimethicone" (USP / NF). Wacker explicitly rules out the use of SILFAR® 100 for parenteral applications. National regulations applicable in the countries concerned must be observed.

Application: SILFAR® 100 is used predominantly in the pharmaceutical sector e.g. as an basic raw material in pharmaceutical formulations.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.959 - 0.965 g/cc0.0346 - 0.0349 lb/in³DIN 57175
Volatiles <= 0.30 %<= 0.30 %
Kinematic Viscosity 95 - 105 cSt95 - 105 cStDIN 53018
 
Thermal PropertiesMetricEnglishComments
Solidus -55.0 °C-67.0 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.402 - 1.4041.402 - 1.404
Transmission, Visible 90 %90 %"Clear" but manufacturer does not quantify.
 
Descriptive Properties
Acidity<5 mg/kgdirect titration
Appearanceclear, colorless and odorless

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PWACK9431 / 204960

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.