MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Sipol Technipol® PA 132 Thermoplastic Adhesive Co-polyamide
Categories: Polymer; Adhesive; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Description: Technipol PA 132 is a thermoplastic adhesive co-polyamide based, principally developed for the shoe industry. It has good flexibility, wettability and adhesion on leather, wood, cardboard. Technipol PA 132 contains around 80 % of raw materials coming from renewable resources (non edible).

Information provided by SIPOL SpA

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.980 g/cc0.0354 lb/in³ASTM D 792
Viscosity  2.25 cP
@Temperature 230 °C
2.25 cP
@Temperature 446 °F
 4.0 cP
@Temperature 210 °C
4.0 cP
@Temperature 410 °F
 6.0 cP
@Temperature 190 °C
6.0 cP
@Temperature 374 °F
 8.0 cP
@Temperature 185 °C
8.0 cP
@Temperature 365 °F
 13 cP
@Temperature 170 °C
13 cP
@Temperature 338 °F
Brookfield Viscosity 6.5 cP
@Temperature 190 °C
6.5 cP
@Temperature 374 °F
Cone/ plate Viscometer, Model Brookfield CAP 2000+.; MI 12
Storage Temperature 5.00 - 10.0 °C41.0 - 50.0 °F
 
Thermal PropertiesMetricEnglishComments
Softening Point 138 °C280 °FASTM D 3461
 
Processing PropertiesMetricEnglishComments
Shelf Life 18.0 Month18.0 Month
 
Descriptive Properties
ColorAmber

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSIPOL008 / 297133

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.